 "id": "ep3tg98gay",
 "slug": "casting-defect",
 "title": "Casting defect",
 "updated": "2026-10-15",
 "topic_path": [
  {
   "id": "technology",
   "label": "Technology and the built world",
   "api_url": "https://www.edgepedia.org/api/v1/topics/technology"
  },
  {
   "id": "technology.engineering",
   "label": "Engineering and manufacturing",
   "api_url": "https://www.edgepedia.org/api/v1/topics/technology.engineering"
  },
  {
   "id": "technology.engineering.manufacturing.processes",
   "label": "Manufacturing processes and fabrication",
   "api_url": "https://www.edgepedia.org/api/v1/topics/technology.engineering.manufacturing.processes"
  },
  {
   "id": "technology.engineering.manufacturing.processes.casting-molding-and-foundry-work",
   "label": "Casting, molding, and foundry work",
   "api_url": "https://www.edgepedia.org/api/v1/topics/technology.engineering.manufacturing.processes.casting-molding-and-foundry-work"
  }
 ],
 "geo": [
  {
   "id": "geo.mena.tbc.technology.engineering.manufacturing.processes",
   "label": "Middle East and North Africa · Before 500 BC: Manufacturing processes and fabrication",
   "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena.tbc.technology.engineering.manufacturing.processes",
   "path": [
    {
     "id": "geo.mena",
     "label": "Middle East and North Africa",
     "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena"
    },
    {
     "id": "geo.mena.tbc",
     "label": "Middle East and North Africa · Before 500 BC",
     "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena.tbc"
    },
    {
     "id": "geo.mena.tbc.technology",
     "label": "Technology and the built world",
     "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena.tbc.technology"
    },
    {
     "id": "geo.mena.tbc.technology.engineering",
     "label": "Engineering and manufacturing",
     "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena.tbc.technology.engineering"
    },
    {
     "id": "geo.mena.tbc.technology.engineering.manufacturing.processes",
     "label": "Manufacturing processes and fabrication",
     "api_url": "https://www.edgepedia.org/api/v1/geo/geo.mena.tbc.technology.engineering.manufacturing.processes"
    }
   ]
  }
 ],
 "excerpt": "A casting defect is an unwanted irregularity in a cast metal part, such as a void, crack, or dimensional error, formed during mold filling or solidification.",
 "snippet": "A casting defect is an unwanted irregularity in a cast metal part, such as a void, crack, or dimensional error, formed during mold filling or solidification.",
 "node": "technology.engineering.manufacturing.processes.casting-molding-and-foundry-work",
 "markdown": "# Casting defect\n\nA casting defect is an unwanted irregularity in a cast metal part, such as a void, crack, missing section, unwanted projection, inclusion, or dimensional error, that forms while the mold is filled or while the casting solidifies and cools.<sup>[1](https://ytdfoundry.com/blog/sand-casting-defects/)</sup> Defects reduce the output of usable castings and increase production cost, and a single defect may result from one clearly defined cause or from a combination of factors.<sup>[2](https://msvs-dei.vlabs.ac.in/msvs-dei/mem103/Unit3lesson5.html)</sup> A casting may reveal certain flaws immediately after it has been cleaned, while other flaws stay hidden beneath the surface and come to light only when machining cuts into it.<sup>[1](https://ytdfoundry.com/blog/sand-casting-defects/)</sup>\n\n| Key fact | Detail |\n|---|---|\n| Standard classification | The International Committee of Foundry Technical Associations identifies seven basic categories: metallic projections, cavities, discontinuities, defective surfaces, incomplete casting, incorrect dimension, and inclusions or structural anomalies<sup>[3](https://dl.asminternational.org/handbooks/edited-volume/27/chapter-abstract/372716/Common-Defects-in-Various-Casting-Processes?redirectedFrom=PDF)</sup> |\n| Origin-based classification | For sand-mold cast irons, defects are grouped by main origin: the sand mixtures used to make the molds, the mold design and casting geometry, and the casting alloy itself<sup>[4](https://www.mdpi.com/2075-4701/12/3/504)</sup> |\n| Gas defects | Round, smooth-walled cavities 0.5 to 4 mm in diameter, generally located in the upper region of the part as-cast<sup>[5](https://61746c6173.investmentcasting.org/casting/defect/gas/index.html)</sup> |\n| Pinholes | Dispersed holes of 1/8 inch (3 mm) or less, caused mainly by hydrogen and nitrogen absorbed in the melt<sup>[6](https://61746c6173.investmentcasting.org/casting/defect/pinholes/index.html)</sup> |\n| Cold shut | A surface imperfection due to unsatisfactory fusion of metal, formed where two metal fronts meet without bonding<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> |\n| Misrun | Metal freezes before the mold cavity is completely filled, leaving an incomplete casting with rounded edges<sup>[8](https://61746c6173.investmentcasting.org/wax/defect/non-fill/index.html)</sup> |\n| Visual acceptance | ASTM A802 provides four levels of acceptance standards for steel casting surfaces, using SCRATA graded reference comparators for texture, roughness, and discontinuities<sup>[9](https://store.astm.org/a0802-19.html)</sup> |\n\n## Classification\n\nSorting casting defects into categories is a hard task, since so many distinct causes contribute and since one and the same defect can show different traits according to the casting's geometry, when in the process it arises, or which foundry produced it.<sup>[4](https://www.mdpi.com/2075-4701/12/3/504)</sup> The International Committee of Foundry Technical Associations groups defects into seven basic categories: metallic projections, cavities, discontinuities, defective surfaces, incomplete casting, incorrect dimension, and inclusions or structural anomalies.<sup>[3](https://dl.asminternational.org/handbooks/edited-volume/27/chapter-abstract/372716/Common-Defects-in-Various-Casting-Processes?redirectedFrom=PDF)</sup> A rough alternative groups defects by broad types of origin, such as those caused by improper mold preparation, pouring practice, or metal chemistry.<sup>[10](https://rmkec.ac.in/tmp/mech/Contents/manufacturingtechnologyI.pdf)</sup>\n\n**Origin-based grouping.** For sand-mold cast irons, one review classifies defects into three classes according to their known main origin: defects related to the sand mixtures used to make the molds, defects associated with the mold design and the geometry of the castings, and defects related to the casting alloy itself. Because of the strong interactions between the melt and the mold during casting, this classification cannot be exact.<sup>[4](https://www.mdpi.com/2075-4701/12/3/504)</sup>\n\n## Porosity defects\n\n**Gas porosity.** [Gas porosity](https://www.edgepedia.org/gas-porosity) is a condition caused by the trapping of gas in the molten metal or by mold gases evolved during pouring.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> In the investment casting atlas, gas defects appear as round, smooth-walled cavities of 0.5 to 4 mm diameter, generally in the upper region of the part as-cast, where rising bubbles are trapped by the solidifying metal. Turbulent flow mixes exiting air with the entering metal, and gas can also come from incomplete burnout of wax and filler material, out-gassing of ceramic cores, or low mold permeability.<sup>[5](https://61746c6173.investmentcasting.org/casting/defect/gas/index.html)</sup> Corrections include adding vents at the top of the part, modifying gating to reduce turbulence, increasing mold permeability or using vacuum assistance, and raising the metal temperature so bubbles have more time to escape before a skin forms.<sup>[5](https://61746c6173.investmentcasting.org/casting/defect/gas/index.html)</sup>\n\n**Pinholes.** Pinholes are dispersed holes of 1/8 inch or less, smaller and more numerous than gas defects, and more common in plain carbon and low alloy steels than in higher alloy steels. They form when gases absorbed during melting, chiefly hydrogen and nitrogen, exceed the solid-state solubility limit and form bubbles during solidification; chemically combined water released from the mold is an alternate mechanism. Remedies include using cleaner or virgin metal, complete degassing, drying ladles and molds, and reducing casting temperature or molten holding time.<sup>[6](https://61746c6173.investmentcasting.org/casting/defect/pinholes/index.html)</sup>\n\n**Shrinkage.** Shrinkage is the contraction of metal in the mold during solidification; the term also describes the resulting defect, such as a shrinkage cavity, which results from poor design, insufficient metal feed, or inadequate feeding.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> Internal shrinkage appears as irregular cavities ranging from small dispersed or linear voids up to large cavities, typically at the casting centerline between gates, in isolated heavy sections, or at sharp internal corners. As solidification progresses, liquid feed metal has increasing difficulty reaching the solidification front, and shrinkage occurs between dendritic arms. Because it is subsurface, internal shrinkage may not be discovered without x-ray examination, machining, or sectioning through the casting; corrections include adequate feeding to promote progressive solidification, insulation to increase the thermal gradient, and hot isostatic pressing to close the defects.<sup>[11](https://61746c6173.investmentcasting.org/casting/defect/shrink-internal/index.html)</sup>\n\nDistinguishing gas porosity from shrinkage porosity matters because the fixes differ: a void can be gas porosity, addressed by fixing the fill, or shrinkage porosity, addressed by fixing the feeding.<sup>[12](https://knowledge.alumcasting.com/reference/casting-defect-catalog/)</sup> Misdiagnosis can itself create defects; if shrinkage porosity is identified as gas porosity and the pouring temperature is lowered, the result may be a cold shut.<sup>[13](https://www.ijies.net/finial-docs/finial-pdf/2905183719.pdf)</sup>\n\n## Filling defects\n\n**Cold shut.** A cold shut is a surface imperfection due to unsatisfactory fusion of metal.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> It takes the form of a crack or discontinuity with rounded edges, indicating that two or more streams of metal froze or solidified before they had time to fuse completely, and it typically appears in thin sections or areas farthest from the gate where two metal fronts meet. Corrections include increasing metal superheat and mold temperature, improving permeability to reduce backpressure, adjusting alloy composition for fluidity, increasing the pour rate, and maintaining a steady pour until the mold is full.<sup>[14](https://61746c6173.investmentcasting.org/wax/defect/cold-shut/index.html)</sup>\n\n**Misrun.** A misrun, also called non-fill or short pour, is an incomplete casting with rounded edges where the metal froze before the mold cavity was completely filled, typically in thin sections and sharp edges away from the gate. Corrections include raising metal and mold temperatures, pouring without interruption, improving fluidity by reducing oxides or adjusting chemistry, venting thin sections, and modifying gating to create more entry points for the alloy.<sup>[8](https://61746c6173.investmentcasting.org/wax/defect/non-fill/index.html)</sup>\n\n## Cracks and tears\n\nA hot tear is a fracture with an irregular form that appears in a casting when internal stress, produced by sharp temperature differences as the metal solidifies, causes it to crack.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> In the investment casting atlas it appears as a jagged crack with an irregular path, typically with an oxidized fracture face, located in slow-to-cool areas where the geometry involves seriously restrained contraction or a local volume of unfed metal, and it may occur at the intersection of thick and thin sections. The stated mechanism is that during cooling the strength of the shell or gating system exceeds that of the solidifying metal. Corrections span casting design, such as adequate fillet radii and avoiding major sectional changes, mold practice, such as reducing mold strength and slowing the cooling rate, and metal chemistry, such as using certified virgin ingots.<sup>[15](https://61746c6173.investmentcasting.org/casting/defect/hot-tear/index.html)</sup>\n\n## Inclusions and surface defects\n\nInclusions are particles of slag, refractory materials, sand, or deoxidation products trapped in the casting during pouring and solidification.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> Sand inclusions are cavities or surface imperfections caused by sand washing into the mold cavity, and slag inclusions contain impurities from charge materials, silica and clay eroded from the refractory lining, and ash from fuel during melting.<sup>[7](https://www.afsinc.org/metalcasting-terms)</sup> Non-metallic inclusions in investment castings generally form smooth-sided irregular negative shapes; ceramic-derived inclusions are more angular and may contain embedded ceramic, and the shape of the defect aids in determining its source.<sup>[16](https://61746c6173.investmentcasting.org/casting/defect/non-metallic-inclusion/index.html)</sup> Slag, being less dense than the metal, floats to the top surface of the casting, and it is difficult to visually distinguish slag from gas defects; inspection under magnification may reveal residual slag.<sup>[17](https://61746c6173.investmentcasting.org/casting/defect/slag/index.html)</sup>\n\nMetallographic examination distinguishes genuine porosity from preparation artifacts: real casting porosity has rounded, smooth interior walls, while pull-out artifacts have irregular, freshly-fractured walls, and grinding-introduced cracks are linear and oriented to the grinding direction.<sup>[18](https://www.metallography.org/guides/castings-foundry-analysis)</sup>\n\n## Inspection and standards\n\nSurface acceptance of steel castings is governed by ASTM A802, which covers acceptance criteria for surface texture, surface roughness, and surface discontinuities by visual examination and provides four levels of acceptance standards. Acceptance levels use Steel Castings Research and Trade Association (SCRATA) graded reference comparators, with levels A through J covering surface texture, nonmetallic inclusions, gas porosity, solidification discontinuities, sand expansion discontinuities, metal inserts, thermally cut surfaces, mechanically prepared surfaces, and welded surfaces.<sup>[9](https://store.astm.org/a0802-19.html)</sup> Radiographic reference standards include ASTM E155 for aluminum and magnesium castings, ASTM E272 for copper-base and nickel-copper alloy castings, and ASTM E446 for steel castings up to 2 in. (51 mm) in thickness.<sup>[18](https://www.metallography.org/guides/castings-foundry-analysis)</sup>\n\n**Systematic diagnosis.** The American Foundry Society teaches a 10-Step Procedure for analyzing and reducing casting defects, from writing a problem statement through building a corrective action plan, supported by training modules on gas-related, oxide-related, sand-related, and shrink-related defects and by the International Atlas of Casting Defects.<sup>[19](https://www.afsinc.org/e-learning/casting-defect-analysis)</sup> Because human visual inspection of cast products is slow and unproductive in mass production, convolutional neural networks have been widely applied to automatic defect detection, though the diversity and variation in defect appearance make the task challenging.<sup>[20](https://arxiv.org/abs/2107.11643)</sup>\n\n## References\n\n1. [Sand Casting Defects: Types, Causes & Prevention, YTD Foundry](https://ytdfoundry.com/blog/sand-casting-defects/)\n2. [Defects in Sand Casting, Manufacturing Processes-I, Virtual Labs](https://msvs-dei.vlabs.ac.in/msvs-dei/mem103/Unit3lesson5.html)\n3. [Rathindra DasGupta, Common Defects in Various Casting Processes, ASM Handbook Vol 15, Casting, 2008, p 1192-1202](https://dl.asminternational.org/handbooks/edited-volume/27/chapter-abstract/372716/Common-Defects-in-Various-Casting-Processes?redirectedFrom=PDF)\n4. [Casting Defects in Sand-Mold Cast Irons: An Illustrated Review, Metals 12(3), 504, MDPI](https://www.mdpi.com/2075-4701/12/3/504)\n5. [Gas, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/gas/index.html)\n6. [Pinholes, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/pinholes/index.html)\n7. [Glossary of Metalcasting Terms, American Foundry Society](https://www.afsinc.org/metalcasting-terms)\n8. [Non Fill (Misrun), Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/wax/defect/non-fill/index.html)\n9. [ASTM A802-19, Standard Practice for Steel Castings, Surface Acceptance Standards, Visual Examination](https://store.astm.org/a0802-19.html)\n10. [Sand Casting Defects, Manufacturing Technology I, RMK Engineering College](https://rmkec.ac.in/tmp/mech/Contents/manufacturingtechnologyI.pdf)\n11. [Shrink - Internal, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/shrink-internal/index.html)\n12. [Casting Defect Catalog: Causes, Identification and Correction, Industrial Manufacturing Knowledge Base](https://knowledge.alumcasting.com/reference/casting-defect-catalog/)\n13. [Defect Identification and Process Optimization in Metal Casting Operation, IJIES](https://www.ijies.net/finial-docs/finial-pdf/2905183719.pdf)\n14. [Cold Shut, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/wax/defect/cold-shut/index.html)\n15. [Hot Tear, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/hot-tear/index.html)\n16. [Non-Metallic Inclusion, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/non-metallic-inclusion/index.html)\n17. [Slag, Atlas of Casting Defects, Investment Casting Institute](https://61746c6173.investmentcasting.org/casting/defect/slag/index.html)\n18. [Castings and Foundry Analysis in Metallography, Metallography.org](https://www.metallography.org/guides/castings-foundry-analysis)\n19. [Casting Defect Analysis e-Learning, American Foundry Society](https://www.afsinc.org/e-learning/casting-defect-analysis)\n20. [An Uncertainty-Aware Deep Learning Framework for Defect Detection in Casting Products, arXiv:2107.11643](https://arxiv.org/abs/2107.11643)\n\n---\n*Topic: Encyclopedia › Technology and the built world › Engineering and manufacturing › Manufacturing processes and fabrication › Casting, molding, and foundry work*\n\n*Initially written Sep 17, 2026 · Reviewed: Oct 15, 2026 · Edited: Oct 15, 2026 · Last review: Oct 15, 2026*\n\n*Copyright 2026 EdgeChat AI, a subsidiary of Biostate AI.*\n\nLicense: Edgepedia Community License 1.0, https://www.edgepedia.org/edgepedia/license\n",
 "same_as": [],
 "url": "https://www.edgepedia.org/casting-defect",
 "markdown_url": "https://www.edgepedia.org/casting-defect.md",
 "license": {
  "name": "Edgepedia Community License 1.0",
  "url": "https://www.edgepedia.org/edgepedia/license",
  "summary": "Free with credit, commercial use included. AI training is open to everyone. For other uses, organizations over USD 100M in revenue or 100M monthly users license separately.",
  "spdx": "LicenseRef-Edgepedia-Community-1.0"
 },
 "credit": "\"Casting defect\", Edgepedia (EdgeChat), https://www.edgepedia.org/casting-defect. Edgepedia Community License 1.0.",
 "credit_md": "\"[Casting defect](https://www.edgepedia.org/casting-defect)\", Edgepedia (EdgeChat), [https://www.edgepedia.org/casting-defect](https://www.edgepedia.org/casting-defect). [Edgepedia Community License 1.0](https://www.edgepedia.org/edgepedia/license).",
 "credit_html": "\"<a href=\"https://www.edgepedia.org/casting-defect\">Casting defect</a>\", Edgepedia (EdgeChat), <a href=\"https://www.edgepedia.org/casting-defect\">https://www.edgepedia.org/casting-defect</a>. <a href=\"https://www.edgepedia.org/edgepedia/license\">Edgepedia Community License 1.0</a>.",
 "speakable": "A casting defect is an unwanted irregularity in a cast metal part, such as a void, crack, or dimensional error, formed during mold filling or solidification."
}