CrCoNi

CrCoNi medium-entropy alloy is an equiatomic chromium, cobalt, and nickel alloy whose strength, ductility, and fracture toughness increase as temperature falls toward liquid helium temperatures.

ferronickel

Ferronickel (FeNi) is an iron-nickel ferroalloy, typically 20 to 40% nickel, produced from laterite ores by the rotary kiln–electric furnace process and used as a stainless steel raw material.

Gamma prime

Gamma prime (γ′) is the ordered intermetallic precipitate, based on Ni₃(Al, Ti), that is the principal strengthening phase in nickel-based superalloys for jet-engine turbine disks and blades.

Gamma titanium aluminide

Gamma titanium aluminide (γ-TiAl) is a lightweight intermetallic alloy with a density of about 4 g/cm³ that retains strength at 650–850 °C, used in jet engine turbine blades.

GRX-810

GRX-810 is an oxide dispersion strengthened NiCoCr medium entropy alloy developed by NASA's Glenn Research Center for 3D printing of rocket engine and turbine parts.

Hastelloy C-276

Hastelloy C-276 is a wrought nickel-chromium-molybdenum-tungsten corrosion-resistant alloy produced by Haynes International, defined in 1965 and widely used in chemical processing and flue gas desulfurization.

Incoloy 825

Incoloy 825, also known as Alloy 825 or UNS N08825, is a nickel-iron-chromium alloy introduced in the 1950s for corrosion resistance, especially to sulfuric acid and sour gas.

Metal foam

A metallic foam is a cellular material of solid metal, often aluminum, filled with gas-filled pores, used in aerospace, automotive, and biomedical engineering for its light weight and energy absorption.

Ni3Al

Ni3Al, or nickel aluminide, is an intermetallic compound of nickel and aluminum best known as the gamma-prime strengthening phase of nickel-based superalloys in turbine engines.

NiAl

NiAl (nickel aluminide) is an intermetallic compound of nickel and aluminum with a high melting point, low density, and excellent oxidation resistance, but brittle at room temperature.

Nimonic

Nimonic is a family of nickel-chromium superalloys strengthened by aluminum and titanium, developed in the United Kingdom during World War II for gas-turbine blades and other high-temperature uses.

Permalloy

Permalloy is a family of soft magnetic nickel–iron alloys, typically about 80% nickel and 20% iron, valued for very high permeability and used in magnetic shielding and sensors.

Single-crystal superalloy

A single-crystal superalloy is a nickel-based high-temperature alloy cast so the entire component, typically a gas turbine blade, forms one crystal with no grain boundaries for exceptional creep strength.

Stellite

Stellite is a family of cobalt-based wear- and corrosion-resistant alloys developed by Elwood Haynes in 1887, used for hardfacing valve seats, pump shafts, and saw tips.

Ultralight metallic microlattice

An ultralight metallic microlattice is a cellular material of hollow metal tubes, developed at HRL Laboratories and reported in 2011, with densities as low as 0.9 mg/cm³.

Waspaloy