# Fracture toughness

**Fracture toughness** is a material property that measures resistance to the extension of a crack: it is the critical value of the stress intensity factor, or of an equivalent parameter such as J or crack-tip opening displacement, at which a pre-existing sharp crack begins to grow rapidly<sup>[1](https://www.unsw.edu.au/science/our-schools/materials/engage-with-us/high-school-students-and-teachers/online-tutorials/crack-theory/fracture-mechanics/fracture-toughness)</sup><sup> • </sup><sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup>. The property underlies flaw-tolerance assessment of pressure vessels, pipelines, aircraft structures, and nuclear components, where the question is not whether a flaw exists but how large a flaw the material can tolerate at a given stress<sup>[3](https://store.astm.org/e0399-20.html)</sup>.

| Key fact | Detail |
|---|---|
| Fracture criterion | Fast fracture occurs when the applied stress intensity factor K reaches the critical value Kc, the fracture toughness<sup>[1](https://www.unsw.edu.au/science/our-schools/materials/engage-with-us/high-school-students-and-teachers/online-tutorials/crack-theory/fracture-mechanics/fracture-toughness)</sup> |
| Governing equation | K = Yσ√(πa), where σ is applied stress, a the crack length, and Y a dimensionless geometry factor<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup> |
| Plane-strain value | KIc, measured under severe tensile constraint with a small crack-tip plastic zone, is treated as a lower limiting toughness for 2% apparent crack extension<sup>[3](https://store.astm.org/e0399-20.html)</sup> |
| Representative values | Steel alloy about 150 MPa√m, aluminum alloy 37, mild steel 50, PMMA 1.1, glass 0.7<sup>[5](https://etd.ohiolink.edu/acprod/odb_etd/ws/send_file/send?accession=osu150185598849201&disposition=inline)</sup> |
| Primary test standards | ASTM E399 for KIc; ASTM E1820 for K, J, and CTOD; ISO 12737 and ISO 12135 are the ISO equivalents<sup>[3](https://store.astm.org/e0399-20.html)</sup><sup> • </sup><sup>[6](https://store.astm.org/e1820-25.html)</sup><sup> • </sup><sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup> |
| Indirect screening | Charpy V-notch impact energy correlates with toughness but does not directly measure it<sup>[7](https://nvlpubs.nist.gov/nistpubs/gcr/2022/NIST.GCR.22-917-51.pdf)</sup> |

## Stress intensity factor and the fracture criterion

A crack concentrates stress. In linear elasticity the stress field ahead of a crack tip has a characteristic form in which the magnitude of the stresses is set by a single parameter, the stress intensity factor K. For a crack of length 2a in an infinite plate under remote stress σ, the factor is K = σ√(πa); in general K = Yσ√(πa), where Y is a dimensionless number that depends on the shape of the body and the distribution of the load<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>. For a small crack in a large body, K is determined mainly by the size of the crack and is comparatively insensitive to the crack's shape<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>.

The fracture criterion follows directly. When K reaches a critical value Kc, the crack extends; this critical value is the toughness of the material<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>. Knowing Kc lets an engineer compute either the crack length that will cause fast fracture at a given applied stress, or the applied stress that will cause fast fracture for a given crack length<sup>[1](https://www.unsw.edu.au/science/our-schools/materials/engage-with-us/high-school-students-and-teachers/online-tutorials/crack-theory/fracture-mechanics/fracture-toughness)</sup>. K is a loading parameter, computed from geometry and load; Kc is a material parameter, determined by a fracture test<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>.

An equivalent energy view defines the energy release rate G, the energy per unit new crack area. For a linear-elastic material under Mode I (opening) loading, J = K²/E′, where E′ equals the Young's modulus E in plane stress and E/(1 − ν²) in plane strain, with ν the [Poisson's ratio](https://www.edgepedia.org/poissons-ratio)<sup>[8](https://mooseframework.inl.gov/releases/moose/2022-06-13/modules/tensor_mechanics/FractureIntegrals.html)</sup>. The critical energy release rate Gc and the critical stress intensity factor Kc are therefore two expressions of the same toughness, related by Gc = Kc²/E′<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>.

## Plane-strain fracture toughness and thickness

Toughness measured on a cracked specimen depends on the stress state at the crack tip, which in turn depends on specimen thickness. Fracture toughness becomes constant for thicknesses exceeding a critical dimension, and this thickness-independent value is the plane-strain fracture toughness, KIc<sup>[9](https://danotes.mech.uwa.edu.au/fracture/plasticity/plasticity.html)</sup>. ASTM E399 defines the conditions: the state of stress near the crack front must approach triaxial plane strain, and the crack-tip plastic zone must be small compared with the crack size, the specimen thickness, and the ligament ahead of the crack<sup>[3](https://store.astm.org/e0399-20.html)</sup>.

Within the allowable range of specimen proportions, KIc can vary, and it may rise with increasing ligament size; nevertheless, the standard treats KIc as a lower limiting value of fracture toughness, taken at 2% apparent crack extension, in the environment and at the speed and temperature of the test<sup>[3](https://store.astm.org/e0399-20.html)</sup>. The E399 procedure is based on crack growth of up to 2% of the specimen width, which can produce a size-dependent rising resistance curve, with larger specimens giving higher results; an optional companion value, KIsi, is based on a fixed 0.5 mm of crack extension and is less sensitive to specimen size<sup>[3](https://store.astm.org/e0399-20.html)</sup>.

The method has defined limits. It does not apply to materials that fail by cleavage fracture, such as ferritic steels in or below the ductile-to-brittle transition region, where crack-front length affects the measurement stochastically; for those, ASTM E1921 and E1820 apply. It also does not apply to high-toughness materials whose failure involves appreciable plasticity<sup>[3](https://store.astm.org/e0399-20.html)</sup>.

## Standard test methods

The basic fracture toughness test subjects a pre-cracked specimen to load in an attempt to initiate crack growth; the material's resistance to that fracture is the measured toughness<sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup>. ASTM E399 determines KIc under predominantly linear-elastic, plane-strain conditions using fatigue-precracked specimens at least 1.6 mm (0.063 in.) thick, loaded with a slowly increasing crack-displacement force<sup>[3](https://store.astm.org/e0399-20.html)</sup>. ISO 12737 is the equivalent ISO method<sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup>.

ASTM E1820 covers the determination of fracture toughness using the parameters K, J, and CTOD (δ), the crack-tip opening displacement, in either R-curve format or as a point value, for Mode I loading. Its recommended specimens are the single-edge bend SE(B), compact C(T), and disk-shaped compact DC(T), all notched and sharpened with fatigue cracks<sup>[6](https://store.astm.org/e1820-25.html)</sup>. Until a revision of the standard, KIc could be evaluated under E1820 as well as E399; to avoid duplication, that evaluation was removed and users are referred to E399<sup>[6](https://store.astm.org/e1820-25.html)</sup>. ISO 12135 is the ISO equivalent of E1820, and ISO 22889 provides guidance for very small, size-sensitive specimens<sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup>.

Material-specific standards supplement these: ASTM B646 is the standard practice for fracture toughness testing of aluminum alloys, B645 is the basic method for plane-strain fracture toughness of aluminum specimens, B909 covers non-stress-relieved aluminum products, and E1304 covers chevron-notched plane-strain testing<sup>[2](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)</sup>. For dynamic or impact loading, ASTM E1221 determines Mode I crack-arrest fracture toughness<sup>[7](https://nvlpubs.nist.gov/nistpubs/gcr/2022/NIST.GCR.22-917-51.pdf)</sup>.

## Values across materials

Fracture toughness varies widely between material classes. Representative values of Kc include about 1 MPa√m for glass and about 100 MPa√m for steel<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>. A tabulation of plane-strain values gives 150 MPa√m for a steel alloy (Gc 107 kJ/m²), 37 MPa√m for an aluminum alloy (20 kJ/m²), 50 MPa√m for mild steel (12 kJ/m²), 1.1 MPa√m for PMMA (0.5 kJ/m²), 1.1 MPa√m for polystyrene (0.4 kJ/m²), and 0.7 MPa√m for glass (0.007 kJ/m²)<sup>[5](https://etd.ohiolink.edu/acprod/odb_etd/ws/send_file/send?accession=osu150185598849201&disposition=inline)</sup>.

The choice of parameter changes rankings. Because Gc = Kc²/E′, dividing by a large modulus compresses differences in Kc: silica is tougher than rubber when ranked by critical stress intensity factor, but rubber is tougher than silica when ranked by fracture energy<sup>[4](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)</sup>.

## Elastic-plastic parameters and service assessment

When a material's failure involves substantial plasticity, the linear-elastic K description no longer applies, and toughness is expressed through J or CTOD. In defect assessment procedures, equivalent K values derived from these parameters are designated KJ or KCTOD to distinguish them from plane-strain KIc<sup>[10](https://www.twi-global.com/technical-knowledge/faqs/faqwhat-is-the-relationship-between-the-fracture-toughness-parameters-k-ctod-and-j)</sup>. E1820 notes that its fracture toughness values serve as a basis for material comparison, selection, quality assurance, and structural flaw tolerance assessment, and that toughness can rank materials within a similar yield strength range<sup>[6](https://store.astm.org/e1820-25.html)</sup>.

Fracture toughness capacity depends not only on the material but also on temperature, rate of load application, and level of stress constraint<sup>[7](https://nvlpubs.nist.gov/nistpubs/gcr/2022/NIST.GCR.22-917-51.pdf)</sup>. Because the standard fracture tests are costly and difficult to perform, toughness capacity is often estimated indirectly from the Charpy V-notch impact test, a high loading-rate test that measures the energy absorbed during fracture; empirical relations relate Charpy energy to KIc and dynamic toughness values, but the Charpy result does not directly measure fracture toughness<sup>[7](https://nvlpubs.nist.gov/nistpubs/gcr/2022/NIST.GCR.22-917-51.pdf)</sup><sup> • </sup><sup>[11](https://www.nist.gov/programs-projects/charpy-machine-verification-program)</sup>.

Applying laboratory toughness values to service components requires accounting for differences between test and field conditions. Cyclic forces can extend cracks at K values below KIc, and crack extension under sustained loads, as in stress corrosion cracking or [creep crack growth](https://www.edgepedia.org/creep-crack-growth), can be influenced by temperature and environment<sup>[3](https://store.astm.org/e0399-20.html)</sup>. Residual stresses can also bias measured KIc values, particularly for specimens taken from as-heat-treated stock, weldments, or products with intentionally induced residual stresses<sup>[3](https://store.astm.org/e0399-20.html)</sup>.

## References

1. [Fracture toughness, UNSW School of Materials Science and Engineering](https://www.unsw.edu.au/science/our-schools/materials/engage-with-us/high-school-students-and-teachers/online-tutorials/crack-theory/fracture-mechanics/fracture-toughness)
2. [Slotwinski, Cooke, Moylan (2012). Mechanical Properties Testing for Metal Parts Made via Additive Manufacturing, NISTIR 7847](https://tsapps.nist.gov/publication/get_pdf.cfm?pub_id=910618)
3. [ASTM E399-20, Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness of Metallic Materials](https://store.astm.org/e0399-20.html)
4. [Suo, Zhigang. ES 247 Fracture Mechanics: Linear Elastic Fracture Mechanics lecture notes](https://imechanica.egr.uh.edu/sites/default/files/Linear%20elastic%20fracture%20mechanics%202014%2003%2008.pdf)
5. [Fracture toughness values table, Ohio State University thesis (OhioLINK ETD)](https://etd.ohiolink.edu/acprod/odb_etd/ws/send_file/send?accession=osu150185598849201&disposition=inline)
6. [ASTM E1820-25, Standard Test Method for Measurement of Fracture Toughness](https://store.astm.org/e1820-25.html)
7. [NIST GCR 22-917-51, Literature Review for PJP Column Splices](https://nvlpubs.nist.gov/nistpubs/gcr/2022/NIST.GCR.22-917-51.pdf)
8. [Fracture Integrals, MOOSE framework documentation](https://mooseframework.inl.gov/releases/moose/2022-06-13/modules/tensor_mechanics/FractureIntegrals.html)
9. [DANotes: Fracture Mechanics, Plasticity](https://danotes.mech.uwa.edu.au/fracture/plasticity/plasticity.html)
10. [What is the relationship between the fracture toughness parameters K, CTOD and J? TWI](https://www.twi-global.com/technical-knowledge/faqs/faqwhat-is-the-relationship-between-the-fracture-toughness-parameters-k-ctod-and-j)
11. [Charpy Machine Verification Program, NIST](https://www.nist.gov/programs-projects/charpy-machine-verification-program)

---
*Initially written Sep 17, 2026 · Reviewed: Sep 17, 2026; Oct 15, 2026 · Edited: Oct 15, 2026 · Last review: Oct 15, 2026*

Topic: Physical world and mathematics › Physics › Classical physics › Mechanics › Continuum, solid, and fluid mechanics › Solid mechanics › Fracture and failure › Fracture mechanics

Copyright 2026 Edgepedia

License: Edgepedia Community License 1.0, https://www.edgepedia.org/edgepedia/license

Source: https://www.edgepedia.org/fracture-toughness