# Pitting corrosion

Pitting corrosion is a form of localized corrosion in which metal dissolves at small points on the surface, forming cavities, as a result of breakdown of the otherwise protective passive film on the metal.<sup>[1](https://www.osti.gov/biblio/653362)</sup> It occurs mainly on metals whose corrosion resistance depends on passivity, and its danger lies in the contrast between a nearly undamaged surface and deep local penetration: pits tend to grow into the metal rather than spread across it, and the severity of attack is difficult to estimate from visual inspection of the surface.<sup>[2](https://discovery.ucl.ac.uk/1557238/1/PhD_Thesis_T.S.Pathan_12092524.pdf)</sup>

| Key fact | Detail |
|---|---|
| Definition | Localized accelerated dissolution of metal caused by breakdown of the otherwise protective passive film, producing cavities confined to points or small areas.<sup>[1](https://www.osti.gov/biblio/653362)</sup><sup> • </sup><sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> |
| Susceptible metals | Predominantly passive metals: aluminum and its alloys, titanium alloys, iron and nickel alloys, and copper and zinc alloys.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup> |
| Aggressive species | Halide ions above a critical concentration, with chloride (Cl⁻) the most common; the main role of chloride is to increase the chance of passive film breakdown rather than to inhibit repassivation.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[5](https://www.sciencedirect.com/science/article/abs/pii/S0169433299003281)</sup> |
| Stages | Passivity breakdown and pit initiation, metastable pitting with repassivation, and stable pit propagation; initiation and propagation are clearly separable processes.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[6](https://www.sciencedirect.com/science/article/pii/S0010938X99000128)</sup> |
| Propagation mechanism | Localized acidification inside the pit (the Galvele model); Hoar proposed an autocatalytic mechanism based on pH drop inside the pit in 1937.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup> |
| Key parameters | Pitting potential (the potential at which the passive film starts to break down locally) and critical pitting temperature (the threshold above which stable pit growth can occur).<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup><sup> • </sup><sup>[7](https://doi.org/10.1016/j.mtcomm.2026.114806)</sup> |
| Standard tests | ASTM G48 (ferric chloride pitting and crevice tests, Methods A–F) and ASTM G61 (cyclic potentiodynamic polarization in chloride environments).<sup>[8](https://store.astm.org/g0048-11r20e01.html)</sup><sup> • </sup><sup>[9](https://store.astm.org/standards/g61)</sup> |

## Where it occurs

Pitting affects metals that resist uniform corrosion by carrying a passive oxide film. The review literature lists aluminum and its alloys, titanium and its alloys, iron and nickel alloys, and copper and zinc alloys as the affected classes.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup> Stainless steels are a typical case: their chromium oxide film protects the surface, and pitting occurs when that film breaks down locally under attack by halide ions such as chloride or fluoride.<sup>[2](https://discovery.ucl.ac.uk/1557238/1/PhD_Thesis_T.S.Pathan_12092524.pdf)</sup>

The environment must supply aggressive anions above a critical concentration. Chloride is the most common pitting agent, and pitting will not occur if there is no localized breakdown of the passive film, for example when the oxide film is completely destroyed and uniform corrosion takes over instead.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[2](https://discovery.ucl.ac.uk/1557238/1/PhD_Thesis_T.S.Pathan_12092524.pdf)</sup> Susceptibility also depends on the alloy itself: the integrity of the oxide film, the presence of inclusions, second-phase particles, pores, grain or phase boundaries, scratches, and other discontinuities, which are the preferred sites for anion adsorption and pit nucleation.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup>

## Stages of the pitting process

**Initiation.** The process begins with localized changes in the passive film. The commonly accepted first step is the localized adsorption of aggressive anions, chiefly chloride, on the passivated surface, often at discontinuities in the film such as inclusions, precipitates, voids, or mechanical damage.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> Many nucleation mechanisms have been proposed over the decades, including chloride penetration through the film (Evans), ion migration and adsorption models (Hoar, Kolotyrkin, Uhlig), film fracture under electrostatic pressure (Sato), and vacancy accumulation at the metal–film interface (Lin, and the point defect model of Chao and colleagues). There is no full agreement among researchers on the mechanism, and passivity breakdown remains the least understood stage of the process.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup><sup> • </sup><sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup>

**Metastable pitting.** Between initiation and stable growth lies an intermediate stage. Metastable pits nucleate and grow for a short time below the critical pitting potential and then repassivate; under potentiostatic control in chloride solutions they appear as fluctuations of current that precede the formation of stable pits.<sup>[6](https://www.sciencedirect.com/science/article/pii/S0010938X99000128)</sup><sup> • </sup><sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup> Because these pits repassivate, their growth is described as metastable. Whether a metastable pit becomes stable depends on how well the repair process competes with local acidification; in Burstein's framing, passivity is in a continuous process of breakdown and repair, and the likelihood of a stable pit is a question of how good the repair is.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup>

**Propagation.** Once a pit stabilizes, dissolution of the underlying bulk metal drives growth. In 1937 Hoar proposed an autocatalytic mechanism in which the main cause of pitting is the drop of pH inside the pit; as the pit develops, chloride concentration increases, local pH decreases, and the environment inside becomes more corrosive, so the attack deepens rather than spreads.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[2](https://discovery.ucl.ac.uk/1557238/1/PhD_Thesis_T.S.Pathan_12092524.pdf)</sup> The pit acts as a local anode, with the cathodic reaction, oxygen reduction, occurring on the surrounding passive surface, and the metal at the pit bottom held in the active dissolution region even at high applied potentials.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[10](https://www.nature.com/articles/s41529-018-0037-2)</sup> Pit cavities vary from shallow to cylindrical, approximately hemispherical shapes, and their morphology depends on the alloy's metallurgy, the solution chemistry, and loading conditions.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> Openings can be very small while large cavities develop beneath the surface.<sup>[11](https://sarjaweb.vtt.fi/julkaisut/muut/2008/081107_A02_16_L_Carpen.pdf)</sup>

## Pitting potential, temperature, and growth rate

The pitting potential is the potential at which the passive film starts to break down locally; below it pits do not nucleate, and above it nucleated pits can grow.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> In general the pitting potential decreases with increasing chloride ion concentration.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> The time from the start of film breakdown to measurable pit formation, the induction time, is a statistical quantity over the whole surface, expressed as 1/τ = k′(E − E<sub>p</sub>), where E is the applied potential and k′ depends on chloride concentration.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup>

Temperature provides a second criterion. The critical pitting temperature (CPT) defines the threshold above which sustained pit propagation can occur at a given electrochemical potential. Below the CPT only metastable pits form and repassivate; above it the passive film breaks down locally and stable growth follows. The transition is governed by the balance between the anodic dissolution current and the diffusion-limited current set by mass transport out of the pit: below the CPT the diffusion-limited current is smaller than the critical passivation current density, and above it the order reverses, allowing stable propagation.<sup>[7](https://doi.org/10.1016/j.mtcomm.2026.114806)</sup>

Pit growth rate depends on temperature, pH, passive film properties, chloride concentration, other ions in solution, and the orientation of the material. A widely used empirical relation from Godard gives pit depth as d = K·t<sup>1/3</sup>; it was developed from data on aluminum but has been observed to hold for other materials in different water environments.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup>

## Testing and ranking alloys

Laboratory standards rank alloy resistance by accelerating initiation relative to natural environments. ASTM G48 exposes specimens to ferric chloride solution through six procedures: Method A (ferric chloride pitting test), Method B (crevice test), and Methods C through F, which rank alloys by the minimum critical temperature needed to initiate pitting or crevice corrosion. Methods A and B are designed to cause breakdown of Type 304 stainless steel at room temperature. The results rank resistance under the specific test conditions and cannot be applied to environments that do not contain chlorides, and no statement about propagation can be made from them.<sup>[8](https://store.astm.org/g0048-11r20e01.html)</sup> Surface preparation matters: grinding or pickling can destroy the passive layer, and 24 hours of air passivation after such treatment is sufficient to minimize the differences.<sup>[8](https://store.astm.org/g0048-11r20e01.html)</sup>

Electrochemical testing complements immersion tests. ASTM G61 covers cyclic potentiodynamic polarization to determine relative susceptibility to localized corrosion for iron-, nickel-, or cobalt-based alloys in chloride environments; the potential at which anodic current rises rapidly indicates susceptibility to initiation, and the potential at which the hysteresis loop closes indicates the likelihood of propagation.<sup>[9](https://store.astm.org/standards/g61)</sup>

## Service performance and failure cases

Alloying level determines field behavior. In a 28-month exposure in the hot chlorinated seawater of a desalination plant flash chamber at 100 °C, the lower-alloyed grades type 316, S31726, and S31803 suffered pitting and crevice corrosion, the 6Mo grade S31254 suffered only superficial crevice corrosion, and the most highly alloyed stainless steel S32654 and the nickel-base alloy N06625 were fully resistant.<sup>[12](https://www.sciencedirect.com/science/article/pii/S0011916499000910)</sup>

Pitting can also strike where conditions look benign. In Finnish power plant fire protection systems, EN 1.4301 and EN 1.4401 stainless steel pipes carrying stagnant tap water with only 21 to 28 mg/l chloride perforated within a few years, with pits located in welds and heat-affected zones. In such low-chloride drinking waters the pitting potential of these steels at room temperature is normally very high, above 1000 mV versus SCE, but microbial colonization raises the open-circuit potential, a process called ennoblement, which can exceed the pit initiation potential even in low-chloride waters. Iron-oxidizing bacteria convert ferrous iron to ferric iron, which reacts with chloride to form ferric chloride, an extremely aggressive pitting agent for austenitic stainless steels. The pit initiation potential on welds and heat-affected zones is lower than on base metal, so pitting often starts there.<sup>[11](https://sarjaweb.vtt.fi/julkaisut/muut/2008/081107_A02_16_L_Carpen.pdf)</sup>

## Consequences beyond metal loss

Pits act as stress concentrators and initiation sites for other failure modes. Under cyclic loading, cracks have been observed to nucleate from pits, and corrosion fatigue models combine pit growth rate theory with linear elastic fracture mechanics to estimate the time for a pit to reach the critical depth at which a fatigue crack forms.<sup>[3](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)</sup> Pitting also connects to stress corrosion cracking: phase-field formulations of dissolution-driven cracking capture both pitting and the pit-to-crack transition through a film rupture–dissolution–repassivation mechanism.<sup>[13](https://arxiv.org/abs/2011.12068)</sup> Because pits are rare, nanometer-scale initiation events with extreme local chemistry changes, predicting where and when they will form remains difficult, and stochastic models using Poisson processes for initiation and Markov or renewal processes for growth are an active area of development.<sup>[4](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)</sup><sup> • </sup><sup>[7](https://doi.org/10.1016/j.mtcomm.2026.114806)</sup>

## References

1. [G. S. Frankel (1998). Pitting corrosion of metals: A review of the critical factors. Journal of the Electrochemical Society.](https://www.osti.gov/biblio/653362)
2. [Electrochemistry of Corrosion, T. S. Pathan PhD thesis, University College London.](https://discovery.ucl.ac.uk/1557238/1/PhD_Thesis_T.S.Pathan_12092524.pdf)
3. [D. W. Hoeppner (2012). Exfoliation Corrosion and Pitting Corrosion and Their Role in Fatigue Predictive Modeling: State-of-the-Art Review. International Journal of Aerospace Engineering.](https://onlinelibrary.wiley.com/doi/10.1155/2012/191879)
4. [Passivity breakdown, pit initiation and propagation of pits in metallic materials – Review. Corrosion Science 90 (2015) 5–22.](https://www.sciencedirect.com/science/article/pii/S0010938X14004533)
5. [The role of chloride ions in pitting of carbon steel studied by the statistical analysis of electrochemical noise. Applied Surface Science.](https://www.sciencedirect.com/science/article/abs/pii/S0169433299003281)
6. [Pitting corrosion of aluminum. Corrosion Science.](https://www.sciencedirect.com/science/article/pii/S0010938X99000128)
7. [Modeling pitting corrosion in stainless steels: A comprehensive review. Materials Today Communications (2026).](https://doi.org/10.1016/j.mtcomm.2026.114806)
8. [ASTM G48-11(2020)e1: Standard Test Methods for Pitting and Crevice Corrosion Resistance of Stainless Steels and Related Alloys by Use of Ferric Chloride Solution.](https://store.astm.org/g0048-11r20e01.html)
9. [ASTM G61-86(2024): Standard Test Method for Conducting Cyclic Potentiodynamic Polarization Measurements for Localized Corrosion Susceptibility of Iron-, Nickel-, or Cobalt-Based Alloys.](https://store.astm.org/standards/g61)
10. [A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals. npj Materials Degradation (2018).](https://www.nature.com/articles/s41529-018-0037-2)
11. [L. Carpen et al. (2008). A case study on corrosion of stainless steel in fire protection systems. VTT.](https://sarjaweb.vtt.fi/julkaisut/muut/2008/081107_A02_16_L_Carpen.pdf)
12. [J. Olsson and K. Minnich (1999). Solid stainless steel for MSF once-through plants. Desalination 124: 85–91.](https://www.sciencedirect.com/science/article/pii/S0011916499000910)
13. [A phase field formulation for dissolution-driven stress corrosion cracking. arXiv:2011.12068.](https://arxiv.org/abs/2011.12068)

---
*Topic: Encyclopedia › Technology and the built world › Engineering and manufacturing › Materials science and metallurgy › Fatigue and fracture*

*Initially written Oct 15, 2026*

*Copyright 2026 EdgeChat AI, a subsidiary of Biostate AI.*

License: Edgepedia Community License 1.0, https://www.edgepedia.org/edgepedia/license