# 磷化钴

磷化钴是钴与磷形成的一类无机化合物，写作Co-P，其中研究最充分的物相包括CoP、Co₂P和CoP₂。这些材料主要用作电解水析氢反应（HER）和析氧反应（OER）的非贵金属电催化剂，同时也用作电池负极材料、锌空气电池阴极催化剂以及加氢脱硫催化剂。<sup>[1](https://pubs.acs.org/accacs/article/15/7/5457/3691739/Applications-of-Cobalt-Phosphide-Based-Materials)</sup>

| 关键事实 | 详情 |
|---|---|
| 主要物相 | CoP、Co₂P和CoP₂，统称Co-P材料<sup>[1](https://pubs.acs.org/accacs/article/15/7/5457/3691739/Applications-of-Cobalt-Phosphide-Based-Materials)</sup> |
| 首次HER报道 | 2014年，沙克及其同事制备了多面体CoP纳米颗粒，在0.5 M H₂SO₄中表现出优异的HER性能<sup>[2](https://www.sciencedirect.com/science/article/pii/S0360319921030238)</sup> |
| 电子结构 | P原子从Co上吸走电子密度，形成部分带正电的Co位点（Coᶛ+）和部分带负电的P位点（Pᶛ−）<sup>[3](https://onlinelibrary.wiley.com/doi/10.1002/ece2.70025)</sup> |
| 基准HER数据 | CoPₓ薄膜在酸中HER的交换电流密度为\( j_0 = -8.9 \times 10^{-5} \) A/cm²，表观活化能为81 ± 15 kJ/mol<sup>[4](https://pubmed.ncbi.nlm.nih.gov/29732273/)</sup> |
| CoP纳米线电解槽 | 对称CoP电极在1.56 V和1.78 V下分别输出10和100 mA cm⁻²，连续运行1000 h无明显衰减<sup>[5](https://www.sciencedirect.com/org/science/article/pii/S2041652017008744)</sup> |
| 电池容量 | CoP作为负极的理论储锂容量为894 mAh g⁻¹<sup>[6](https://pubmed.ncbi.nlm.nih.gov/40889748/)</sup> |
| 钠容量 | 约1000 mAh g⁻¹，嵌钠电位低于0.3 V<sup>[7](https://onlinelibrary.wiley.com/doi/10.1007/s12598-024-03190-x)</sup> |

## 组成与电子结构

磷化钴属于过渡金属磷化物（TMPs），即非贵金属与磷结合而成的一类化合物。磷之所以能改善催化行为，可以从静电角度理解：磷的电负性高于钴，会从钴上吸走电子密度，从而在表面产生部分带正电的钴位点和部分带负电的磷位点。带正电的Coᶛ+位点有利于水或氢氧根离子的吸附，而带负电的Pᶛ−位点可作为质子受体，促进析氢反应的Volmer步骤。<sup>[3](https://onlinelibrary.wiley.com/doi/10.1002/ece2.70025)</sup> 在碱性体系中，钴位点常充当氢化物受体，磷中心则促进质子吸附，这种双位点机制使其本征活性高于许多其他非贵金属催化剂。<sup>[8](https://doi.org/10.1007/s44371-026-00555-2)</sup>

磷化钴之所以受重视，是因为它兼具地壳储量丰富的组成、高电导率、可观的催化活性和合理的稳定性。<sup>[9](https://www.sciencedirect.com/science/article/pii/S2468606921000630)</sup> 其电子结构被认为与铂有一定相似性，这正是它被用作析氢中铂替代材料的基础。<sup>[3](https://onlinelibrary.wiley.com/doi/10.1002/ece2.70025)</sup>

## 电解水催化

电化学电解水将间歇性可再生电力转化为氢燃料，由两个半反应组成：阴极析氢反应和阳极析氧反应。<sup>[10](https://www.sciencedirect.com/science/article/pii/S258996512200023X)</sup> 磷化钴因其高催化活性和耐久性而成为该领域极具潜力的催化剂，研究热度持续不减——在2021年一篇综述发表前的三年间，每年关于CoP基电催化剂的论文数量均超过100篇。<sup>[2](https://www.sciencedirect.com/science/article/pii/S0360319921030238)</sup>

**单一形貌基准。** 气相–固相合成在多孔钴泡沫上制备了单晶CoP纳米线。在OER条件下，纳米线通过电化学原位氧化和脱磷逐步、保形地转化为CoOOH，氧化后的电极在1.0 M KOH中于300 mV过电位（驱动反应所需超出理论最低值的额外电压）下输出100 mA cm⁻²，塔菲尔斜率为78 mV dec⁻¹。同一电极达到−100 mA cm⁻²的HER所需过电位为244 mV，由其构建的对称双电极电解槽在1.56 V和1.78 V下分别输出10和100 mA cm⁻²，并在20和100 mA cm⁻²下运行1000 h无明显衰减。<sup>[5](https://www.sciencedirect.com/org/science/article/pii/S2041652017008744)</sup> 电沉积钴磷衍生薄膜在碱性介质中HER过电位94 mV、OER过电位345 mV时达到10 mA cm⁻²，并以100%法拉第效率驱动全解水。<sup>[11](https://digitalcommons.usu.edu/chem_facpub/679/)</sup>

**掺杂与复合设计。** 性能可通过调节组成和结构来调控。负载在氮掺杂碳上的轻度铜掺杂材料Cu₀.₃Co₂.₇P，在10 mA cm⁻²下OER过电位为0.19 V、HER过电位为0.22 V；用成对的Cu₀.₃Co₂.₇P/NC电极组装的自制电解槽在1.74 V下电流密度比Pt/RuO₂电极对高60%，50 h后失活可忽略。<sup>[12](https://www.pnnl.gov/publications/bimetallic-cobalt-based-phosphide-zeolitic-imidazolate-framework-copx-phase-dependent)</sup> 该领域的综述将主要优化手段归纳为杂原子掺杂、复合构建、与良导电基底集成以及结构调控。<sup>[10](https://www.sciencedirect.com/science/article/pii/S258996512200023X)</sup>

## 稳定性与衰减

稳定性是该领域的核心隐忧。详细的电解后研究表明，电流–电位扫描中表现出的电化学稳定性可能掩盖了巨大的组成变化。一项针对热磷化Co₂P的模型研究发现，该化合物在酸中按化学计量比溶解，在碱性条件下则降解为氢氧化物；碱性电解后其电化学表面积几乎翻倍，电解液分析显示碱性电解液中磷优先于钴溶解。<sup>[13](https://pubs.acs.org/doi/10.1021/acsenergylett.8b00514)</sup> 另一项针对CoP的研究发现，磷比钴更易浸出，使CoP相转变为Co(OH)₂并提高HER过电位。<sup>[14](https://pubs.acs.org/chreay/article/124/9/5617/154697/Precious-Metal-Free-Hydrogen-Evolution-Catalyst)</sup> 酸性电解中的薄膜CoPₓ电极同样表明，溶解主要经由化学途径进行，反复线性扫描处理会加速腐蚀。<sup>[15](https://pmc.ncbi.nlm.nih.gov/articles/PMC5915747/)</sup>

在OER的强阳极电位下，磷化钴表面通常原位重构为（氧）氢氧化物，后者被广泛认为是OER的真正活性相。转变后的层可能比原始磷化物更具活性，但相变会导致结构退化、活性位点损失或电导率下降，从而影响长期稳定性。<sup>[3](https://onlinelibrary.wiley.com/doi/10.1002/ece2.70025)</sup> 间歇运行还带来另一种失效模式：碱性电解槽停机时，阴极电位升高，趋近于CoPₓ氧化为钴、Co(OH)₂、CoOₓ和CoPₓOᵧ的平衡电位，由此不可逆地生成氧化物和氢氧化物，使HER动力学变差。为缓解这一衰减，研究者设计了一种将电极电位保持在Co(OH)₂平衡电位以下的阴极保护方法。<sup>[16](https://pubs.rsc.org/en/content/articlehtml/2021/ta/d1ta01181b)</sup>

## 电池及其他应用

作为负极材料，CoP通过转化反应形成Li₃P来储存锂，这赋予其高比容量和离子电导率，且极化仅约0.4 V，小于氧化物（约0.9 V）和硫化物（约0.7 V）。其缺点是本征电导率差以及充放电循环中体积膨胀显著。<sup>[6](https://pubmed.ncbi.nlm.nih.gov/40889748/)</sup><sup> • </sup><sup>[17](https://www.sciencedirect.com/science/article/pii/S1674200123002389)</sup> 对于钠离子电池，磷化钴因其约1000 mAh g⁻¹的理论容量和低于0.3 V的嵌钠电位而颇具吸引力。<sup>[7](https://onlinelibrary.wiley.com/doi/10.1007/s12598-024-03190-x)</sup> 磷化钴及其衍生物还被评估用作锌空气电池的空气阴极催化剂，在高正电位下磷化钴原位氧化生成的钴氧化物贡献OER活性，而杂原子掺杂碳则支撑氧还原反应。<sup>[18](https://www.sciencedirect.com/science/article/pii/S2352152X24031311)</sup><sup> • </sup><sup>[19](https://pubs.rsc.org/en/content/articlepdf/2025/cc/d4cc05498a)</sup>

在储能之外，钴镍磷化物还被探索用作加氢脱硫的加氢处理催化剂——即从原油原料中脱除硫——其中CoₓNi₂−ₓPᵧ/SiO₂的活性被归因于相对于磷化镍而言表面磷的富集。<sup>[20](https://www.sciencedirect.com/science/article/pii/S0021951708003771)</sup>

## 合成

已报道的路线涵盖多种方法。CoP纳米颗粒可通过两步胶体法制备：在230 °C下由八羰基二钴在油胺、1-十八烯和壬酸中形成钴纳米颗粒，然后与三辛基膦在约330 °C下反应转化为CoP。<sup>[21](https://www.sciencedirect.com/science/article/pii/S221128551630091X)</sup> 其他方法包括水热合成后磷化处理制备纳米片，<sup>[22](https://www.sciencedirect.com/science/article/abs/pii/S0169433225002491)</sup> 氧化物薄膜的气相热磷化（例如用PH₃处理等离子体增强原子层沉积的Co₃O₄），<sup>[4](https://pubmed.ncbi.nlm.nih.gov/29732273/)</sup> 钴泡沫上纳米线的气相–固相生长，<sup>[5](https://www.sciencedirect.com/org/science/article/pii/S2041652017008744)</sup> 钴磷薄膜的电沉积，<sup>[11](https://digitalcommons.usu.edu/chem_facpub/679/)</sup> 以及表面团簇的化学气相沉积。<sup>[23](https://advanced.onlinelibrary.wiley.com/doi/10.1002/advs.202520390)</sup>

## References

1. [Applications of Cobalt Phosphide-Based Materials in Electrocatalysis, ACS Catalysis (2025)](https://pubs.acs.org/accacs/article/15/7/5457/3691739/Applications-of-Cobalt-Phosphide-Based-Materials)
2. [Recent progress in CoP-based materials for electrochemical water splitting, International Journal of Hydrogen Energy (2021)](https://www.sciencedirect.com/science/article/pii/S0360319921030238)
3. [Cobalt-Based Catalysts for Electrochemical Water Splitting: A Review of Mechanisms, Performance, and Applications, EcoEnergy (2025)](https://onlinelibrary.wiley.com/doi/10.1002/ece2.70025)
4. [Stability of CoPx Electrocatalysts in Continuous and Interrupted Acidic Electrolysis of Water, ChemElectroChem (2018)](https://pubmed.ncbi.nlm.nih.gov/29732273/)
5. [Vapor–solid synthesis of monolithic single-crystalline CoP nanowire electrodes for efficient and robust water electrolysis, Chemical Science (2017)](https://www.sciencedirect.com/org/science/article/pii/S2041652017008744)
6. [Recent Progress on CoP as Anodes for Metal-Ion Batteries (2025)](https://pubmed.ncbi.nlm.nih.gov/40889748/)
7. [A review on phosphorus and metal phosphides as anodes for sodium-ion batteries, Rare Metals (2025)](https://onlinelibrary.wiley.com/doi/10.1007/s12598-024-03190-x)
8. [Non-noble metal catalysts for the alkaline hydrogen evolution reaction: a review, Discover Chemistry (2026)](https://doi.org/10.1007/s44371-026-00555-2)
9. [Advances in CoP electrocatalysts for water splitting, Materials Today Energy (2021)](https://www.sciencedirect.com/science/article/pii/S2468606921000630)
10. [Recent advances in cobalt phosphide-based materials for electrocatalytic water splitting, Nano Materials Science (2024)](https://www.sciencedirect.com/science/article/pii/S258996512200023X)
11. [Electrodeposited Cobalt-Phosphorous-Derived Films as Competent Bifunctional Catalysts for Overall Water Splitting, Angewandte Chemie (2015)](https://digitalcommons.usu.edu/chem_facpub/679/)
12. [Bimetallic Cobalt-Based Phosphide Zeolitic Imidazolate Framework, Advanced Energy Materials (2017), PNNL record](https://www.pnnl.gov/publications/bimetallic-cobalt-based-phosphide-zeolitic-imidazolate-framework-copx-phase-dependent)
13. [Evaluating the Stability of Co2P Electrocatalysts in the Hydrogen Evolution Reaction for Both Acidic and Alkaline Electrolytes, ACS Energy Letters (2018)](https://pubs.acs.org/doi/10.1021/acsenergylett.8b00514)
14. [Precious Metal Free Hydrogen Evolution Catalyst Design and Application, Chemical Reviews (2024)](https://pubs.acs.org/chreay/article/124/9/5617/154697/Precious-Metal-Free-Hydrogen-Evolution-Catalyst)
15. [Stability of CoPx Electrocatalysts in Continuous and Interrupted Acidic Electrolysis of Water, PMC full text (2018)](https://pmc.ncbi.nlm.nih.gov/articles/PMC5915747/)
16. [Sacrificial species approach to designing robust transition metal phosphide cathodes for alkaline water electrolysis in discontinuous operation, Journal of Materials Chemistry A (2021)](https://pubs.rsc.org/en/content/articlehtml/2021/ta/d1ta01181b)
17. [Cobalt phosphide-based composites as anodes for lithium-ion batteries, Particuology (2024)](https://www.sciencedirect.com/science/article/pii/S1674200123002389)
18. [Advanced cobalt phosphide and derivatives air-cathode catalysts for zinc-air batteries, Journal of Energy Storage (2024)](https://www.sciencedirect.com/science/article/pii/S2352152X24031311)
19. [Transition metal phosphide-based oxygen electrocatalysts for aqueous zinc–air batteries, Chemical Science (2025)](https://pubs.rsc.org/en/content/articlepdf/2025/cc/d4cc05498a)
20. [Hydrodesulfurization properties of cobalt–nickel phosphide catalysts: Ni-rich materials are highly active, Journal of Catalysis (2008)](https://www.sciencedirect.com/science/article/pii/S0021951708003771)
21. [Activity and stability of cobalt phosphides for hydrogen evolution upon water splitting, Nano Energy (2016)](https://www.sciencedirect.com/science/article/pii/S221128551630091X)
22. [Spindle-shaped porous cobalt phosphide ultrathin nanosheets as bifunctional electrocatalysts for water splitting, Applied Surface Science (2025)](https://www.sciencedirect.com/science/article/abs/pii/S0169433225002491)
23. [Modulating Local Electronic Structure via Cluster Engineering on Cobalt Phosphide for Efficient Water/Seawater Splitting, Advanced Science (2026)](https://advanced.onlinelibrary.wiley.com/doi/10.1002/advs.202520390)

---
*Initially written Oct 22, 2026*

Topic: 物质世界与数学 › 化学 › 元素与无机物 › Halides, nitrides, and carbides

Copyright 2026 Edgepedia

License: Edgepedia Community License 1.0, https://www.edgepedia.org/edgepedia/license

Source: https://www.edgepedia.org/zh/cobalt-phosphide

English original: https://www.edgepedia.org/cobalt-phosphide