# 铁六氰合铁酸盐正极

铁六氰合铁酸盐（FeHCF）正极是一种用于钠离子和钾离子电池的普鲁士蓝类似物电极材料，其结构基于开放的立方骨架，其中氰根配体桥接铁中心，而Na+等碱金属离子占据较大的间隙位。铁六氰合铁酸盐是普鲁士蓝本身的另一个名称，即Fe4[Fe(CN)6]3·14H2O，是六氰合铁酸盐（HCF）家族的母体化合物。<sup>[1](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)</sup><sup> • </sup><sup>[2](https://www.taylorfrancis.com/chapters/edit/10.1201/9781003308744-4/prussian-blue-analogues-cathode-materials-sodium-ion-bateries-yinzhu-jiang-yao-huang-yuting-gao)</sup>

| 关键事实 | 详情 |
|---|---|
| 母体结构 | 普鲁士蓝，Fe4[Fe(CN)6]3·14H2O，立方面心Fm-3m；氰根配体桥接高自旋和低自旋铁中心<sup>[1](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)</sup> |
| 通式 | AxM1[M2(CN)6]1−y·zH2O（0 ≤ x ≤ 2，0 ≤ y ≤ 1），其中y为[M2(CN)6]空位分数<sup>[1](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)</sup> |
| 性能范围 | 六氰合铁酸盐在钠离子和钾离子电池中于2.5–3.8 V下可提供70–170 mAh/g的容量<sup>[4](https://advanced.onlinelibrary.wiley.com/doi/10.1002/aenm.202000943)</sup> |
| 富钠目标 | Na2FeFe(CN)6每化学式单元脱出两个Na+，理论容量约170 mAh/g<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup> |
| 主要缺陷 | [Fe(CN)6]空位和配位水，会减少储钠位点、降低电子电导率并减慢Na+扩散；HCF含水量为10–15 wt%<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup> |
| 里程碑材料 | 空气稳定的菱方R-Na1.92Fe[Fe(CN)6]，2015年报道，作为可规模化、低成本的钠离子正极<sup>[6](https://pubmed.ncbi.nlm.nih.gov/25615887/)</sup> |
| 规模化验证 | 配位工程化Fe-HCF在10 kg级反应器中制备：5 C下99.3 mAh/g，100 C下51 mAh/g，50 C下循环超过15,000次<sup>[7](https://pmc.ncbi.nlm.nih.gov/articles/PMC11295058/)</sup> |

## 结构与氧化还原机制

传统普鲁士蓝骨架采用类似钙钛矿的立方面心Fm-3m结构，其中氰根配体桥接高自旋（HS）和低自旋（LS）铁中心。缺失[Fe(CN)6]单元形成的空位每化学式单元可容纳14个水分子，其中6个为与不饱和HS-Fe3+结合的配位水，8个为结构空隙中的晶格水。<sup>[1](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)</sup>在储能组成中，通式为AxM1[M2(CN)6]1−y·zH2O，其中A为碱金属阳离子，M1和M2为通过N和C与氰根配位的过渡金属；空位分数y应尽量降低，因为空位会去除电化学活性位点。<sup>[1](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)</sup>

对于FeHCF正极，储钠通过Fe2+/Fe3+氧化还原电对进行，Na+离子嵌入和脱出开放骨架的大A位。在Na2FeFe(CN)6中，约170 mAh/g的理论容量对应每化学式单元脱出两个Na+离子。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>骨架的大间隙空间正是其适用于钠的根本原因：Na+的离子半径为1.02 Å，摩尔质量为23 g/mol，而Li+为0.76 Å和7 g/mol，因此钠会使许多锂宿主结构发生畸变，需要具有更大间隙空间的宿主。<sup>[8](https://www.sciencedirect.com/science/article/pii/S001085452200073X)</sup><sup> • </sup><sup>[9](https://patentimages.storage.googleapis.com/ac/48/29/211dbcea2a9631/US9099718.pdf)</sup>

结构的钠含量和水含量决定其相行为。当钠分布不均匀时，结构可从立方相转变为单斜相，晶胞体积膨胀6.5%；去除结晶水可减弱泡利排斥，从而实现向更畸变的菱方相的转变。NaxMnHCF和NaxCoHCF中也发生类似的相变，由钠离子和水分子含量驱动。<sup>[3](https://onlinelibrary.wiley.com/doi/full/10.1002/smll.202401957)</sup>

## 作为电池材料的历史

过渡金属六氰合铁酸盐最初作为锂离子电池正极宿主被研究，但锂离子太小，与骨架间隙空间不匹配，导致嵌入过程中容量迅速衰减。2004年，埃夫特哈里将铁六氰合铁酸盐（普鲁士蓝）用作钾离子电池正极，以钾金属为对电极，钾离子尺寸几乎是锂的两倍，与间隙空间匹配良好，可逆容量约75 mAh/g，保持率良好。<sup>[9](https://patentimages.storage.googleapis.com/ac/48/29/211dbcea2a9631/US9099718.pdf)</sup>崔课题组随后研究了水系电解质中铜和镍六氰合铁酸盐的钠、钾和铵嵌入，但水的窄电化学窗口限制了能量密度。<sup>[9](https://patentimages.storage.googleapis.com/ac/48/29/211dbcea2a9631/US9099718.pdf)</sup>

**2015年钠里程碑。** 古迪纳夫课题组与美国夏普实验室合作，报道了一种空气稳定的钠铁六氰合铁酸盐R-Na1.92Fe[Fe(CN)6]，具有菱方结构，被验证为可规模化、低成本的正极，具有高容量、长循环寿命和良好的倍率性能。基于同步辐射的软X射线吸收谱阐明了铁氧化还原循环机制。成功制备高钠离子浓度的脱水铁六氰合铁酸盐进一步使得构建不使用金属钠负极的放电态钠离子电池成为可能，并可在现有锂离子制造基础设施上测试。<sup>[6](https://pubmed.ncbi.nlm.nih.gov/25615887/)</sup><sup> • </sup><sup>[3](https://onlinelibrary.wiley.com/doi/full/10.1002/smll.202401957)</sup>

## 合成挑战：空位与水

核心实际问题是，高性能仅在具有完美晶体结构和开放离子传输骨架的理想电极中才能实现，而这在实际制备中难以达到。合成过程中的快速沉淀会在晶体结构内产生有害空位和间隙水，这些缺陷损害结构完整性、减少Na+储存位点、降低电子电导率并减慢Na+扩散。<sup>[3](https://onlinelibrary.wiley.com/doi/full/10.1002/smll.202401957)</sup><sup> • </sup><sup>[7](https://pmc.ncbi.nlm.nih.gov/articles/PMC11295058/)</sup>六氰合铁酸盐因其晶体结构而固有地含有水，在立方或单斜形式中水含量可达10–15 wt%。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>

**控制策略。** 产物的钠含量取决于前驱体溶液中的钠和过渡金属（尤其是铁）的价态。多种手段可提高钠含量和结晶度：<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>

- 过量钠盐如NaCl营造富钠环境，减少[Fe(CN)6]4−空位和结晶水；一种具有分级结构的富钠Na1.58Fe[Fe(CN)6]0.92即以此法制备。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>
- 螯合剂如柠檬酸钠控制结晶速率并抑制缺陷形成；柠檬酸钠还作为额外钠源。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>
- 表面活性剂如聚乙烯吡咯烷酮（PVP）降低表面张力，减少空位和配位水数量。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>
- 抗坏血酸作为还原剂在惰性N2气氛下抑制Fe2+/[FeII(CN)6]4−氧化为Fe3+/[FeIII(CN)6]3−，实现每化学式单元掺入1.63个钠离子。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>
- 热处理去除结晶水，改善初始容量、循环稳定性和倍率性能。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>

由于完全消除空位仍然困难，且产率较低，研究已转向空位修复策略，包括球磨和高浓度溶液处理。球磨制备的NaFeFe(CN)6显示出空位修复和性能增强，高浓度氯化钠溶液中的亚铁氰化钠已被用于填充表面空位。<sup>[5](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)</sup>

## 工程化FeHCF正极的性能

配位工程——在成核和生长过程中控制配位环境——已产生一些报道中最强的结果。在10 kg级化学反应器中合成的富钠Fe-HCF在5 C（1 C = 100 mA/g）下可逆容量为99.3 mAh/g，即使在100 C下仍为51 mAh/g，50 C下寿命超过15,000次循环，初始库仑效率高达92.7%。将该正极与硬碳负极配对的全电池在1,000次循环后容量保持98.3%，库仑效率维持在100%。<sup>[7](https://pmc.ncbi.nlm.nih.gov/articles/PMC11295058/)</sup>该工作针对的两个固有缺点是贫钠状态和高配位水含量，否则会导致初始库仑效率低和倍率性能差。<sup>[7](https://pmc.ncbi.nlm.nih.gov/articles/PMC11295058/)</sup>

更简单的路线同样有效：自下而上法制备的富钠立方Na1.74Fe[Fe(CN)6]0.90·2.07H2O已被报道为与硬碳负极配对用于低成本储能的候选材料。<sup>[10](https://www.sciencedirect.com/science/article/pii/S0378775321010521)</sup>复合设计解决了同类材料的相关弱点；例如，三层FeHCF@MnHCF@FeHCF核壳结构利用低应变铁六氰合铁酸盐壳层稳定钠锰六氰合铁酸盐，抵抗循环过程中的姜-泰勒畸变。<sup>[11](https://www.sciencedirect.com/science/article/abs/pii/S2352152X25000209)</sup>

## 降解与副反应

气体析出是已记录的失效模式。切亚等人报道，在乙腈中于0.586 V vs. Fc+/Fc下六氰合铁酸盐的不可逆电化学氧化会析出氰气(CN)2，对应约3.93 V vs. Na+/Na，接近[普鲁士白](https://www.edgepedia.org/zh/prussian-white)电池中观察到的(CN)2析出起始电位。提出的机制为ECE型反应，其中电化学形成的Fe4+中间体通过两个氰根配体的还原消除释放(CN)2，随后溶剂、水或氢氧根取代缺失的配体，与铁配位。<sup>[12](https://d-nb.info/1317997166/34)</sup>循环过程中正极颗粒表面也可能形成贫氰层，循环后锰六氰合铁酸盐正极的[X射线衍射](https://www.edgepedia.org/zh/x-ray-diffraction)显示形成NaMnCl3，归因于NaClO4电解质盐的还原。<sup>[12](https://d-nb.info/1317997166/34)</sup>

## 在钠离子正极中的地位

与层状氧化物和聚阴离子化合物相比，FeHCF家族竞争的是成本和倍率而非能量密度。

## References

1. [Prussian Blue Analogues for Non-Aqueous Sodium-Ion and Potassium-Ion Batteries: The Landscape From Lab-Scale Optimizations Toward Practical Applications (Mei et al., Small, 2026)](https://onlinelibrary.wiley.com/doi/10.1002/smll.202514168)
2. [Prussian Blue Analogues as Cathode Materials for Sodium-Ion Batteries (Jiang, Huang, Gao, book chapter)](https://www.taylorfrancis.com/chapters/edit/10.1201/9781003308744-4/prussian-blue-analogues-cathode-materials-sodium-ion-bateries-yinzhu-jiang-yao-huang-yuting-gao)
3. [Prussian Blue Analogues for Sodium-Ion Battery Cathodes: A Review of Mechanistic Insights, Current Challenges, and Future Pathways (Xiao et al., Small, 2024)](https://onlinelibrary.wiley.com/doi/full/10.1002/smll.202401957)
4. [Hexacyanoferrate-Type Prussian Blue Analogs: Principles and Advances Toward High-Performance Sodium and Potassium Ion Batteries (Zhou et al., Advanced Energy Materials, 2021)](https://advanced.onlinelibrary.wiley.com/doi/10.1002/aenm.202000943)
5. [Prussian Blue Analogues for Sodium-Ion Battery Cathodes (Xiao et al., Small, 2024, open repository PDF)](https://opus.lib.uts.edu.au/bitstream/10453/184089/2/Small%20-%202024%20-%20Xiao%20-%20Prussian%20Blue%20Analogues%20for%20Sodium%E2%80%90Ion%20Battery%20Cathodes%20%20A%20Review%20of%20Mechanistic%20Insights%20%20Current.pdf)
6. [Rhombohedral prussian white as cathode for rechargeable sodium-ion batteries (Wang et al., JACS, 2015)](https://pubmed.ncbi.nlm.nih.gov/25615887/)
7. [Coordination engineering for iron-based hexacyanoferrate as a high-stability cathode for sodium-ion batteries (PMC)](https://pmc.ncbi.nlm.nih.gov/articles/PMC11295058/)
8. [Recent progress of Prussian blue analogues as cathode materials for nonaqueous sodium-ion batteries (ScienceDirect)](https://www.sciencedirect.com/science/article/pii/S001085452200073X)
9. [US Patent 9,099,718: Transition-metal hexacyanoferrate cathode battery](https://patentimages.storage.googleapis.com/ac/48/29/211dbcea2a9631/US9099718.pdf)
10. [Facile synthesis and cycling performance maintenance of iron hexacyanoferrate cathode for sodium-ion battery (ScienceDirect)](https://www.sciencedirect.com/science/article/pii/S0378775321010521)
11. [Innovative three-layered FeHCF@MnHCF@FeHCF core-shell design for enhanced sodium-ion battery cathode performance (ScienceDirect)](https://www.sciencedirect.com/science/article/abs/pii/S2352152X25000209)
12. [Elucidating Gas Evolution of Prussian White Cathodes for Sodium-ion Battery Application (d-nb.info)](https://d-nb.info/1317997166/34)
13. [Sodium-ion battery development since 2020 with future perspectives (RSC, J. Mater. Chem. A)](https://pubs.rsc.org/en/content/articlepdf/2026/ta/d5ta07726e)

---
*Initially written Oct 15, 2026*

Topic: 技术与人造世界 › 能源技术 › 电池与储能 › 电池材料与组件 › 钠离子正极材料

Copyright 2026 Edgepedia

License: Edgepedia Community License 1.0, https://www.edgepedia.org/edgepedia/license

Source: https://www.edgepedia.org/zh/iron-hexacyanoferrate-cathode